Notes on the process

Normalization of 1095 steel

1.Heat the blade to 1475 celcius

2.Hold this temperature for between 5 to 10 minutes for thin blades which has been bevelled to a 80% edge.

3.Quenchoil for fast cooling. Quench with a cutting movement into the oil.

Rockwell 57-63 mellom 59 og 61 🙂